Wednesday, June 24, 2020

Re: [MW:31031] Qualification

No not all 

On Wed, Jun 24, 2020, 08:47 Jayadeep C <jayadeepmechanical@gmail.com> wrote:
If one welder qualified in CS, possible to weld SS and Low alloy


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/39ea0722-5eda-4e38-8f5f-873032810eb4n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPRS9UNhJdLUC8Ev-Psii6xH-9R1MwBTDBkemwBtk%2BiHs%3DTKWA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS