Wednesday, June 24, 2020

Re: [MW:31024] 3 Cycle PWHT requirements acc.to ASME

Thanks for your support.


Regarding PWHT of 3 cycles.

Below I have mentioned my PQR ranges for PWHT.

POST WELD HEAT TREATMENT( QW-407)
TEMPERATURE RANGE 630 ±10° C
SOAKING PERIOD 190Min
HEATING RATE 190°C/Hours Max
COOLING RATE 190°C/Hours Max.
As per the above range, it's qualified 3 cycles, but how? and for 3 Cycles PWHT where I required test coupons? how many coupons tests shall I have conduct?
Please clarify my above query in detail with code.

Thanks once again.

Kiran


On Tuesday, June 23, 2020 at 11:43:19 AM UTC+5:30, petervsoloman wrote:
Dear Kiran,
Once PWHT competed for joints due to modification cut/reweld or repair re PWHT required that particular joints.
it is mention in the procedure is enough to do the job. This you can mention in your weld repair procedure.
Regards,
PETER SOLOMAN
+971 33663119

On Mon, Jun 22, 2020 at 7:32 AM K K <kara...@gmail.com> wrote:
Dear All,

Please describe to me regarding 3 cycle PWHT requirements as per ASME.

If my PQR tested with two coupons where I required one more test coupon and additional one more for repair.

Please explain to me in detail and related to mechanical testing for PWHT.

What is the meaning of this paragraph - **an additional one PWHT cycle shall be incorporated to simulate field repair or modification.**

Thanks and Regards
Kiran

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2b255cdf-b673-4981-8fcf-ad1fb4863ecbo%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/66851acd-b858-47d4-9858-4231b68fa30ao%40googlegroups.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...