Wednesday, June 24, 2020

Re: [MW:31023] Qualification

Hi,
Regarding Base material qualification is OK (But please refer QW 423.1)
For Filler metal,position etc., please refer ASME Sec.IX-QW 350,351, Table QW-352 to 357 for essential variables for welder qualification and QW-360 to QW-363 for Welding Operator Qualifications.
Thanks& Regards,

 

(Karthik)

Karthikeyan.S

M: +66-892512282
E-mail : karthik6684@yahoo.com



On Wednesday, June 24, 2020, 10:17:15 AM GMT+7, Jayadeep C <jayadeepmechanical@gmail.com> wrote:


If one welder qualified in CS, possible to weld SS and Low alloy


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/39ea0722-5eda-4e38-8f5f-873032810eb4n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1301932360.1991658.1592969030360%40mail.yahoo.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...