Thursday, June 18, 2020

Re: [MW:31015] PWHT for fillet welds ASME B 31.3

Ilkin, the criteria requirements ASME B 31.3 ED 2018
 fillet weld: the throat 




Em sex., 12 de jun. de 2020 às 07:20, Ilkin Hasanov <ilkinhasanov.91@gmail.com> escreveu:
Hi Gents 
Could you please advise are there any requirements for PWHT of fillet welds asper ASME B 31.3 ?


Regards, 
Ilkin Hasanov

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADrxeDYy1_AmnHNMtBWM48rpC827G52WPSFvyt7SUwg%3D3%2BOy6g%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2Bf3b1iST0G1%3DA%2Bg0LPFA5L2b3FL%3DrbPYvZ8Kp%2BVsob0wnvN0A%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...