Re: [MW:31012] Impact subsize specimen thickness

you have to take size only mention in astm 370 bcuse astm mention temp reduction for that subsize for other subsize not mention in astm 370 how you will you decide temp reduction than what is use of code there will be some reason behind each nd every restriction mention in code

On Thu, 11 Jun 2020, 7:38 am ABHISHEK SINGH, <mech.abhi17@gmail.com> wrote:
Dear Experts,

As per ASTM A370 below thickness subsize impact  specimen mentioned are:

10 x 7.5, 10 x 6.7, 10 x 5, 10 x 3.3, 10 x 2.5

Now my question are, if I am taking a sample size of 10 x 4.5. Is it acceptable?

Regards
Abhishek Singh
+917827309480

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/6cbf4b52-1b7d-43a6-958c-b3180c1a10b5o%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOWr6k8Rfs9eGgM5Bo7m5JqVHTsM%2BjdsPnTc%3DiH-nWeHerWgmQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...