Re: [MW:31010] HIC requirement in SS316

HIC is not Applicable for CRA.

Inline image


Thanks & Regards

J.Gerald Jayakumar

0091-6382552037



On Tuesday, June 16, 2020, 10:28:04 AM GMT+7, Vivek Mane <vivek12787@gmail.com> wrote:


Dear Experts,

Kindly share your views on whether the HIC test is done on SS 316 material.
If yes then for which temperature/service it is done. Also give reference to any code/reference.
Thank you in advance.

Regards,
Vivek V.Mane
BVIL Mumbai
08693002244

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAK4-NK81SzbxxvYiB0CSRAs1nN75VE8FfOOHL-Y%3D5g3MyCdqAg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...