Saturday, June 13, 2020

Re: [MW:30998] Impact subsize specimen thickness

dear sir 
you cant use that size reffer only subsize mention in code

On Thu, 11 Jun 2020, 7:38 am ABHISHEK SINGH, <mech.abhi17@gmail.com> wrote:
Dear Experts,

As per ASTM A370 below thickness subsize impact  specimen mentioned are:

10 x 7.5, 10 x 6.7, 10 x 5, 10 x 3.3, 10 x 2.5

Now my question are, if I am taking a sample size of 10 x 4.5. Is it acceptable?

Regards
Abhishek Singh
+917827309480

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/6cbf4b52-1b7d-43a6-958c-b3180c1a10b5o%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOWr6k_b44dYTNjqLXk0owgffwUe834q%2BZwfXYBvgGbfPUg59g%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...