Re: [MW:30998] Filler rod selection for SS 304L to SA 335 pipe welding

Gents,
GTAW - ERNiCr-3
SMAW - ENiCrFe-3

On Saturday, 13 June 2020, 07:58:19 GMT+1, Aakash <harenathjha@gmail.com> wrote:


Hello,
Please suggest what should be the filler rod/ electrode for SS 304L to SA 335 pipe welding by gtaw and smaw process?