Re: [MW:30997] Filler rod selection for SS 304L to SA 335 pipe welding

Prolonged and High temp, NiCrMo3 may not be suitable

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Sat, Jun 13, 2020 at 12:40 PM 'Karthik' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Hi,
Use ENiCrFe-2 or ENiCrMo-3

Thanks& Regards,

 

(Karthik)

Karthikeyan.S

M: +66-892512282
E-mail : karthik6684@yahoo.com



On Saturday, June 13, 2020, 01:58:15 PM GMT+7, Aakash <harenathjha@gmail.com> wrote:


Hello,
Please suggest what should be the filler rod/ electrode for SS 304L to SA 335 pipe welding by gtaw and smaw process?

Regards

--
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/375117352.159368.1592032147808%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNFEQTnVZzcANOGeKmEOgZzYGX%2B9ACL5P4tV%3D9mhyqdZQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...