Re: [MW:30996] Filler rod selection for SS 304L to SA 335 pipe welding

Hi,
Use ENiCrFe-2 or ENiCrMo-3

Thanks& Regards,

 

(Karthik)

Karthikeyan.S

M: +66-892512282
E-mail : karthik6684@yahoo.com



On Saturday, June 13, 2020, 01:58:15 PM GMT+7, Aakash <harenathjha@gmail.com> wrote:


Hello,
Please suggest what should be the filler rod/ electrode for SS 304L to SA 335 pipe welding by gtaw and smaw process?

Regards

--
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c172ae1a-a0a6-4c7f-94e5-413fe1437324o%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/375117352.159368.1592032147808%40mail.yahoo.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...