[MW:31071] Re: 3 Cycle PWHT requirements acc.to ASME

Thanks all for your response to my query.

These requirements as per our contractor specification.
But I need clarification about normal PWHT ( As per B31.3 ) and 3 cycles PWHT, for time calculation.
Thanks once again.

On Monday, June 22, 2020 at 10:02:58 AM UTC+5:30, K K wrote:
Dear All,

Please describe to me regarding 3 cycle PWHT requirements as per ASME.

If my PQR tested with two coupons where I required one more test coupon and additional one more for repair.

Please explain to me in detail and related to mechanical testing for PWHT.

What is the meaning of this paragraph - **an additional one PWHT cycle shall be incorporated to simulate field repair or modification.**

Thanks and Regards
Kiran

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3d9bfe80-783d-4fa4-b161-4e80cde66952o%40googlegroups.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...