[MW:31011] Re: Impact subsize specimen thickness

Dear Mr. Abhishek, 
you can  take sub size specimen provided the specimen size shall not fall below 80% the actual thickness of test coupon . i.e if you are taking specimen against each welding process involved shall not be below 80% of weld deposit @ Test temperature 

if you are not able to take specimen within 80% of test coupon or each weld deposit , you need to apply temperature reduction as per code for size of the specimen you have taken


Regards,
Srinuvasarao
+971 564675865


On Thursday, June 11, 2020 at 7:38:10 AM UTC+4, ABHISHEK SINGH wrote:
Dear Experts,

As per ASTM A370 below thickness subsize impact  specimen mentioned are:

10 x 7.5, 10 x 6.7, 10 x 5, 10 x 3.3, 10 x 2.5

Now my question are, if I am taking a sample size of 10 x 4.5. Is it acceptable?

Regards
Abhishek Singh
+917827309480

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1e9b4125-df8f-47cc-b5f9-f75343a6a3cao%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...