Saturday, June 13, 2020

[MW:30994] HFW pipe line

Dear All.

We have ordered some HFW pipeline for our sour project, which thickness of material is 7.1mm  and manufacturing process shall meet App H&K of API 5L.

Now with considering to API's requirement which UT advised for this pipe, I want to know is it possible to detect LAMINATION by UT or not? 

Regards.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5ee41674-7fbd-4c4b-b224-12a8eb6e3ac2o%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS