Dear

I have a question about my Inspection Certificate of pipe fitting.
We order of material for low temperature ASTM A420 Gr. WPL6.
But, in hard stamp and certificate is "WPL6/WPB" (Attached)
Where i know, for WPB is ASTM A234.
what is the product can used for Low Temperature Service -45degree Celcius???
and if true, any one know reference from standard ASTM???

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4d83d7bf-10a1-4d0e-8cb7-6a0efd0c7679%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...