[MW:28712] Weld metal build up to restore size-

Raw material--- C45 steel
, What is welding produre to build up for restoring required sizes
1, Filler metal,
2, Preheat and interpass, post heat temp
3. Before welding , raw material is to annealed or not??
4. After completion of welding, Any Heat treatment like Normalizing, Quenching and Tempering. 
urgent pl .

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ASNT-Level II in PT,MT,RT & UT.
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35754] interpration

  Interpretation #: BPV IX-18-34  Record Number: 18-771  Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...