Dear ,
this is (P No.8 G No. 4)  to (P No 8 G No. 1)
try with welding wire ER-NiCrMo-3
impact is related to construction code you are using , corrosion also depending on the Requirements of project Spec. 

Regards ,
Ahmed Osman



On Tuesday, December 18, 2018, 5:42:11 a.m. GMT+3, Airion <eomsy81@gmail.com> wrote:


dear all

i would like to get many comments from everyone who have been experienced  making a pWPS.

i have a S31254 pipe [4" sch.40 (t=6mm) ]  and S31603 pipe [4"sch.40 (t=6mm)

is it alight the material spec. for all of tests for ? ex) impact test, penetrant test, bend test, hardness test, corrosion test, macro,micro test, tensil test .

please give your value advice.

thank you

SY Eom


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...