Greetings,

SA194 nuts has not placed any assigned P no as per ASME IX and also with ASME II does not say about welding, still welding of non service requirements does not fall under projects requirements which can be welded with SA 36 plate fabricated to pipe, if your SA194 grades are 1, 2 , 2HM and 2H only. if not you have to qualify procedure.

Officially SA194 nuts are not indended for welding, check safety factors.

Other members views also are highly appreciated.

Thanks.


Regards,
Mohamed Muneeb Mahaboob
CSWIP 3.2-89247/2 
ASNT-NDT-L2-RTFI-RT-UT-MT-PT.
SAP#:70021650 APs:JAPID, QCS & QCI.
muneebslsa@gmail.com +91-636-955-7189

62:8) Say, "Indeed, the death from which you flee - indeed, it will meet you. Then you will be returned to the Knower of the unseen and the witnessed, and He will inform you about what you used to do.".

 
Date: 2018-12-05 14:48
Subject: [MW:28733] SA 194 nut to SA 36 plate fabricated pipe WPS
Dear Expert,

Is there any separate  wps required for welding  SA 194 nuts with SA 36 fabricated pipe.nut is used only for the support the insulation .shall be use 

Regards,
Deepu c

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...