Monday, December 17, 2018

Re: [MW:28784] Aws D1.1

Hi Chandra,
1- Yes, he is qualified for fillet welds on pipes regardless of the pipe diameter. Table4.10 - Check note " f " for joint shapes.
2- Shielding gas is not an essential variable for the welders. Changing the composition of the gas is an essential variable for FCAW-G for prequalified WPS and for PQR as well. Check table 3.1 & 4.5

On Mon, Dec 17, 2018 at 3:04 PM Chandra <chandrasekhar.palapala@gmail.com> wrote:
Boxbe This message is eligible for Automatic Cleanup! (chandrasekhar.palapala@gmail.com) Add cleanup rule | More info
Hi all,
I have few questions regarding AWS D1.1.

1. If a welder qualifies on 3G and 4F
He is qualified for all positions on fillet welds.

Is he qualify on pipe fillet weld? What  Diameter limits he can weld on fillet.

2. If a welder qualifies the welding process FCAW using mix gas (80%Ar +20%CO2)
Can he weld FCAW process using 100% CO2?

Please suggest ...


Best Regards,
Chandra

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
Thanks & Regards
Hisham Al. Mohammad
Welding Engineer & QA/QC Engineer
Mob: +971 56 433 7326 & +971 52 667 9935

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...