[MW:28790] Re: LIMIT OF WELDER QUALIFICATION OVER DIA. RANGE

Dear Friend,
As per code ,Joint Design- Any Groove,Pipe Diameter-Any,Pipe Thickness-Any.So he qualified any diameter and thickness of fillet weld.


Regards,
Binit Kumar

On Wednesday, August 13, 2008 at 1:41:02 PM UTC+5:30, shailesh dave wrote:
DEAR MEMBERS,
 
I HAVE COME ACROSS AN INTERESTING SITUATION.
 
WE HAVE WELDERS QUALIFIED IN 6" x 7.11 mm THK. PIPE OFF COURSE BUTT WELD. MY QUESTION IS CAN THESE WELDER PERFORM WELDING OF SMALL BORE PIPE LIKE 3/4" SOCKET WELD.
 
PL. HELP ME.
 
REGARDS,
 
S.N.DAVE
 
QA/QC INCHARGE
ADGAS, DAS ISLAND, UAE

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...