Hi Darshan,

 

What's  the weld overlay in question?

Please refer the following clause of ISO-15156-3, Part 3: Cracking-resistant CRAs (corrosion resistant alloys) and other alloys. Hardness for weld overlays has to match the respective hardness requirement for the CRA in question.

Annex-A provides the design conditions and acceptance criteria, including hardness restriction for various types of CRA's. Hardness for the weld overlays should match that of the base meta(CRA) in question.

 

 

Thanks.

 

P.Goswami.P.Eng, IWE.

Independent Welding & Metallurgical Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@quickclic.net,pradip.goswami@gmail.com

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Revdiwala Darshan
Sent: December 24, 2018 9:10 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:28809] Hardness requirment for CRO as per ISO 15156

 

Clause 7.3 address hardness of  BM & HAZ, there is no specific hardness  acceptance value mentioned for WOL Material.

On Mon, 24 Dec 2018, 10:35 am muneebslsa@gmail.com, <muneebslsa@gmail.com> wrote:

Greetings,

 

Check para 7.3 and A.13, also refer below TWI page. 

 

 

Thanks.


Regards,

Mohamed Muneeb Mahaboob

CSWIP 3.2-89247/2 

IRCA-9001:2015 LA

ASNT-NDT-L2-RTFI-RT-UT-MT-PT.

SAP#:70021650 APs:JAPID, QCS & QCI.

muneebslsa@gmail.com M +91-636-955-7189

''If you know any art by any means then SCULPT IT - no matter how cheap or useless it is - JUST SCULPT IT, you will never know when experts will be on demand'' 

 

Date: 2018-12-20 11:33

Subject: [MW:28798] Hardness requirment for CRO as per ISO 15156

Dear Experts,

Can anybody explain weld overlay hardness requirment as per NACE MR0175/ISO 15156.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...