Re: [MW:28778] Request for Welding Consumable for Kanthal(R) AF Material

Dear Shaji,
Can you please provide more details about the alloy ?!

Thanks and regards
Hisham Almetwally

On Sun, 16 Dec 2018, 5:44 pm 'shaji nair' via Materials & Welding <materials-welding@googlegroups.com wrote:
Boxbe This message is eligible for Automatic Cleanup! (materials-welding@googlegroups.com) Add cleanup rule | More info
Dear Sir,

Request to guide me the SMAW electrode to use Kanthal® AF Ferritic iron-chromium-aluminium alloy (FeCrAl alloy).

At present we are planning to use 670 electrode with SMAW process.

Request for your guidance.

Thanks & Regards,

Shaji Nair

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...