Friday, December 28, 2018

[MW:28823] Use of ss309 electrode in cracked area

Dear experts
Whether it is advisable to use ss309 electrode to arrest the crack in mild steel material .As my job is fully machined it is difficult to completely remove the crack.kindly guide me.

--