Monday, December 17, 2018

Re: [MW:28780] RE: 28775] Request for Welding Consumable for Kanthal® AF Material

Hi,

In addtion to that refer attached data.

Thanks.

Regards,
Mohamed Muneeb Mahaboob
CSWIP 3.2-89247/2 
IRCA-9001:2015 LA
ASNT-NDT-L2-RTFI-RT-UT-MT-PT.
SAP#:70021650 APs:JAPID, QCS & QCI.
muneebslsa@gmail.com +91-636-955-7189
''If you know any art by any means then SCULPT IT - no matter how cheap or useless it is - JUST SCULPT ITyou will never know when experts will be on demand'' 
 
Sender: PGoswami
Send Time: 2018-12-17 06:36
Subject: [MW:28777] RE: 28775] Request for Welding Consumable for Kanthal® AF Material

Shaji,

 

There's very little information available for this alloy. Originally this product belonged to Sandvik, now it's a separate company. I've attached some information. The highlighted text in the first attachment may be of help.

You may ask Sandvik or their  agents for further help. I'm not sure what is 670 electrode, hence can't make any comment about its suitability.

 

Let me know if it helps.

 

Thanks.

 

P.Goswami.P.Eng, IWE.

Independent Welding & Metallurgical Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@quickclic.net,pradip.goswami@gmail.com

 

From: 'shaji nair' via Materials & Welding [mailto:materials-welding@googlegroups.com]
Sent: December 16, 2018 8:32 AM
To: Pradip Goswami <pradip.goswami@gmail.com>
Cc: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:28775] Request for Welding Consumable for Kanthal® AF Material

 

Dear Sir,

 

Request to guide me the SMAW electrode to use Kanthal® AF Ferritic iron-chromium-aluminium alloy (FeCrAl alloy).

 

At present we are planning to use 670 electrode with SMAW process.

 

Request for your guidance.

 

Thanks & Regards,

 

Shaji Nair

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...