Re: [MW:28804] Material certification EN 3.1 OR 3.2 ?

Dear Shaikh,

4.2 Inspection certificate 3.2 "type 3.2"
Document prepared by both the manufacturer's authorized inspection representative, independent of the manufacturing department and either the purchaser's authorized inspection representative or the inspector designated by the official regulations and in which they declare that the products supplied are in compliance with the requirements of the order and in which test results are supplied.
It shall be permissible for the manufacturer to transfer on to the inspection certificate 3.2 relevant test results
obtained by specific inspection on primary or incoming products he uses, provided that the manufacturer operates
traceability procedures and can provide the corresponding inspection documents required.

Hence as per your shot 3.2 certification required.
-----
Thanks & Regards,

Umesh 



On Mon, Dec 24, 2018 at 4:09 PM shaikh ahmed <ahmedmech77@gmail.com> wrote:
Dear Expert,

Please can you advise on below snap shot of Specification asking for EN 3.2 Material certification correct me ?

it calling for EN 3.2 OR 3.1

image.png

thanks.
Ahmed

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...