Re: Re: [MW:28735] LR BEND TO LR BEND WELDING IN PIPELINE AS PER API1104

Long radius bend to LR bend allowed? 

Yes, if your designer approves.

Thanks.


Regards,
Mohamed Muneeb Mahaboob
CSWIP 3.2-89247/2 
ASNT-NDT-L2-RTFI-RT-UT-MT-PT.
SAP#:70021650 APs:JAPID, QCS & QCI.
muneebslsa@gmail.com +91-636-955-7189

(62:8) Say, "Indeed, the death from which you flee - indeed, it will meet you. Then you will be returned to the Knower of the unseen and the witnessed, and He will inform you about what you used to do."

 
From: Anil Kumar
Date: 2018-12-05 13:58
Subject: Re: [MW:28732] LR BEND TO LR BEND WELDING IN PIPELINE AS PER API1104
I think  you are asking about cold bending operation, and welding of joints between two bend sections, it is allowed as,"extremities of each joint remain straight over a minimum distance of 2 m or twice the pipe diameter, whichever is greater" . this is referred from SP 1208 Pipeline Construction specification (PDO Specfication).

Thanks & Regards,

Bathula Anil Kumar

PH N0: +91-7675019922



On Wed, Dec 5, 2018 at 6:35 AM Mohit <mohitmechlion@gmail.com> wrote:
Dear all,

Can we perform welding directly LR Bend to LR Bend in pipeline ??

Refer to code API 1104.

Joint is before to IJ(Isolation Joint) at Intermediate Pigging Station.

Thanx in advance.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...