Thursday, December 20, 2018

Re: [MW:28796] Material Certification for PUMP as per EIL Standard or API Standard EN10204-3.1 / 3.2/2.2--EIL India

Hi
Based on the criticality rating of the equipment's, the material certification requirements are decided.

Refer the pump MR (Maternal Specification), project purchase material specification / pump data sheet, there you can get the complete information.

Regards
P Govindan

On Dec 20, 2018 6:51 AM, "shaikh ahmed" <ahmedmech77@gmail.com> wrote:
Dear Experts,

Material Certification for PUMP components as per EIL Standard or API Standard  ( whether it is EN10204-3.1 / 3.2/2.2 for Pump components)

Please can you advise in which EIL Standard or API standard  to find the material certification requirement for Pump whether it is require   EN3.1 or 3.2 or 2.2 for Pumps various components in EIL Specification or API Standard

waiting for your response.

thanks.
Ahmed

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...