basically code says about pwht but heat treatment cycle is same as pwht and in pwht only weld seam is consider but is stress relieving only material is consider mainly name is different process is same but focus point is same ( weld joint in pwht and base metal in sr ).
for fibre elongation u can go upto 40% for P1 material

--