Dear Sir,
-- If PQR is Qualified with ASTM A 572 Gr.50 To ASTM A 572 Gr.50( Group no II) for FCAW process.
1) Can I mentioned in WPS as a AWS Group No - I & II Equivalent Unlisted ?
2) And i have received WPS with comments from one of my client ,( The comment is like Unlisted materials not allowed by pre qualified WPS)
Please explain me regarding Unlisted material.
I am looking your valuable replay on my above query.
Regards
Kiran