Hi,
To understand in whole for the preparation of WQTR, you check some of the forms in ANNEX M, which has WQTR forms, which will give you an understanding and preparation of WQTR forms.
If you read 4.18, it directs to 4.8 and your case shall be contemplated as per 4.8.3.
Please check below for how base metal range has qualified for welder.
Thanks.
Regards,
Mohamed Muneeb Mahaboob
CSWIP 3.2-89247/2
IRCA-9001:2015 LA
ASNT-NDT-L2-RTFI-RT-UT-MT-PT.
SAP#:70021650 APs:JAPID, QCS & QCI.
''If you know any art by any means then SCULPT IT - no matter how cheap or useless it is - JUST SCULPT IT, you will never know when experts will be on demand''
Its annex n?--On 15 Dec 2018 8:16 a.m., "muneebslsa@gmail.com" <muneebslsa@gmail.com> wrote:--Check ANNEX M.
Regards,Mohamed Muneeb MahaboobCSWIP 3.2-89247/2IRCA-9001:2015 LAASNT-NDT-L2-RTFI-RT-UT-MT-PT.SAP#:70021650 APs:JAPID, QCS & QCI.''If you know any art by any means then SCULPT IT - no matter how cheap or useless it is - JUST SCULPT IT, you will never know when experts will be on demand'' - MUNEEB-Dear All,--I need some clarification as below.1) GMAW Process WPS and PQR Qualified with A36 -Group no- I. Can I mentioned in WQTR range qualify with Group No-I,II,III and IV.2) SMAW Process - Can I Mentioned In WPS range as what i Mentioned in table.
PQR
WPS range
1
Specification No
A 5.1-04
A 5.1
2
AWS No
E-7018
E 6010 / E 7018
3
Filler No
4
1,2,.3,4
4
Analysis No
1
1
5
polarity
AC(+)
AC & DC
Please if any thing wrong please let me know with AWS D1.1 Standard.Kiran
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com .
Visit this group at https://groups.google.com/group/materials-welding .
For more options, visit https://groups.google.com/d/optout .
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com .
Visit this group at https://groups.google.com/group/materials-welding .
For more options, visit https://groups.google.com/d/optout .
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Comments