Re: [MW:28784] Aws D1.1

Hi,
For Question 2, Table 4.12 and Annex M(Example of WPQR) will give clear answer.
 
Regards
ABDUL MUNEER M
+966550216718 (KSA)
+919895480850 (IND)


On Mon, Dec 17, 2018 at 2:55 PM muneebslsa@gmail.com <muneebslsa@gmail.com> wrote:
Hi Palapala,

1) Read Table 4.10.
&
2) 5.3.

Thanks.


Regards,
Mohamed Muneeb Mahaboob
CSWIP 3.2-89247/2 
IRCA-9001:2015 LA
ASNT-NDT-L2-RTFI-RT-UT-MT-PT.
SAP#:70021650 APs:JAPID, QCS & QCI.
muneebslsa@gmail.com +91-636-955-7189
''If you know any art by any means then SCULPT IT - no matter how cheap or useless it is - JUST SCULPT ITyou will never know when experts will be on demand'' 
 
From: Chandra
Date: 2018-12-17 16:58
Subject: [MW:28782] Aws D1.1
Hi all,
I have few questions regarding AWS D1.1.
 
1. If a welder qualifies on 3G and 4F
He is qualified for all positions on fillet welds.
Is he qualify on pipe fillet weld? What  Diameter limits he can weld on fillet.
 
2. If a welder qualifies the welding process FCAW using mix gas (80%Ar +20%CO2)
Can he weld FCAW process using 100% CO2?
 
Please suggest ...
 
 
Best Regards,
Chandra
 
--
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...