Re: [MW:28804] Material certification EN 3.1 OR 3.2 ?

Hi
MTC's are normally a 3.1 certificate, however we could not judge with above snapshot, it is a 3.1 or 3.2 certificate.


With Kind Regards

P Govindan 


On Mon, Dec 24, 2018 at 1:39 PM shaikh ahmed <ahmedmech77@gmail.com> wrote:
Dear Expert,

Please can you advise on below snap shot of Specification asking for EN 3.2 Material certification correct me ?

it calling for EN 3.2 OR 3.1

image.png

thanks.
Ahmed

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...