Greetings,

AWS materials approved for prequalified welding procedure specification are listed in Table 3.1 of AWS D1.1 according to their ASTM specification. Both parent materials and consumables are also classified in four groups, in AWS D1.1 Table 3.2, depending of their AWS classification and strength, to give guidance for matching strength with the base metal in the case of prequalified welding procedures. In accordance with Table 4.8 all materials unlisted shall be qualified in conformance with clause 4 of the welding procedure qualification of AWS D1.1.


In the case of prequalified welding procedures only material listed in the four groups of Table 3.1 of AWS D1.1 can be used. Table 4.8 specifies that requalification will be necessary if the material selected do not fall within the range qualified. The use of unlisted base metal is restricted to approval.


Thanks.


Regards,
Mohamed Muneeb Mahaboob
CSWIP 3.2-89247/2 
IRCA-9001:2015 LA
ASNT-NDT-L2-RTFI-RT-UT-MT-PT.
SAP#:70021650 APs:JAPID, QCS & QCI.
muneebslsa@gmail.com +91-636-955-7189
''If you know any art by any means then SCULPT IT - no matter how cheap or useless it is - JUST SCULPT ITyou will never know when experts will be on demand'' 
 
From: Kiran
Date: 2018-12-24 11:20
Subject: [MW:28799] As per AWS D1.1-2015
Dear Sir,

If PQR is Qualified with ASTM A 572 Gr.50 To ASTM A 572 Gr.50( Group no II) for FCAW process.

1) Can I mentioned in WPS as a AWS Group No - I & II  Equivalent Unlisted ?

2) And i have received WPS with comments from one of my client ,( The comment is like Unlisted materials not allowed by pre qualified WPS)

Please explain me regarding Unlisted material.

I am looking your valuable replay on my above query.

Regards
Kiran

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...