Monday, December 24, 2018

Re: [MW:28806] Material certification EN 3.1 OR 3.2 ?

Greetings,

Your below clause mandating 3.2.

Differences between EN 10204-3.1 and 3.2 for the MTC

EN 10204 contains 4 types of document type, 2.1, 2.2, 3.1 and 3.2. Type 2.1 and 2.2 are validated by the manufacturer. Type 3.1 and 3.2 are not only validated by manufacturer.
Type 2.1, The content is statement of compliance with the order. Validated by manufacturer.
Type 2.2, Statement of compliance with the order, with indication of results of non specific inspection. Validated by manufacturer.
Type 3.1, Statement of compliance with the order, with indication of results of specific inspection. Authorized inspection representative by the manufacturer, but is independent of the manufacturing department.
Type 3.2, Statement of compliance with the order, with indication of results of specific inspection. Authorized inspection representative by the manufacturer, independent of manufacturing department and either the buyer's authorized inspection representative or the inspector designated by the official regulations.

Thanks

Regards,
Mohamed Muneeb Mahaboob
CSWIP 3.2-89247/2 
IRCA-9001:2015 LA
ASNT-NDT-L2-RTFI-RT-UT-MT-PT.
SAP#:70021650 APs:JAPID, QCS & QCI.
muneebslsa@gmail.com +91-636-955-7189
''If you know any art by any means then SCULPT IT - no matter how cheap or useless it is - JUST SCULPT ITyou will never know when experts will be on demand'' 
 
Date: 2018-12-24 16:56
Subject: [MW:28803] Material certification EN 3.1 OR 3.2 ?
Dear Expert,

Please can you advise on below snap shot of Specification asking for EN 3.2 Material certification correct me ?

it calling for EN 3.2 OR 3.1



thanks.
Ahmed

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...