In my opinion, Heat input is a crucial criteria to achieve impact values in Weld, HAZ and Parent Metal. Travel speed is one of important contributor  for determining heat input. Again it is very important , which material , thickness and welding process used for establishing heat input to achieve desired toughness property. 

You need to referred your historical  records in order to judge and establish heat input parameters to achieve particular range of impact values in given material.

Regards,

Paresh

On Thu, Aug 23, 2018 at 4:35 PM BHIWANDKAR C R <crbhiwandkar.smspl@gmail.com> wrote:
SIR,
WHILE PREPARING WPS THE CONSIDERATION OF 
HEAT INPUT JOULES TO JOULES ON MILL T C
IS REQUIRED TO BE DONE. OR THE TRAVEL SPEED
CAN BE DETERMIND ON THE BASIS OF THE IMAPACT
TEST VALUES GIVEN ON MILL TC

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon

Hi As its %elongation is very low  Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...