Re: [MW:28216] Can I use P NO-1, G NO-1 (PLATE) TO P NO-1, G NO-2 (PLATE) P.Q.R. for welding of ASTM A333 Gr.6 (P No: 1, Group No: 1) to ASTM A350 Gr.LF2 CL.1 (P No: 1, Group No: 2).

You can...provided that the qualifications is available for P.No.1 G No. 1 to itself and P.No.1 G.No.2 to itself and without any change in essential and supplementary essential variables, except group no.....kindly see QW-403.5..

On Fri 24 Aug, 2018, 6:47 PM chiranjeevulu temburu, <chiranjeevi1214@gmail.com> wrote:
Dear All,

Can I use P NO-1, G NO-1 (PLATE) TO P NO-1, G NO-2 (PLATE)  P.Q.R.  for welding of  ASTM A333 Gr.6 (P No: 1, Group No: 1) to ASTM A350 Gr.LF2 CL.1 (P No: 1, Group No: 2).

Please give suggestions in accordance with ASME Section-IX 



Thanks and Best Regards,

CHIRANJEEVULU TEMBURU l +918790956353.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...