Re: [MW:28209] Minimize concavity of fillet weld in saw welding.

thank you for your suggestion but sir, we have already done this, but there is no significant changes.

On Thursday, 23 August 2018 12:29:38 UTC+5:30, kannayeram gnanapandithan wrote:
increase current and reduce travel speed. 

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ASNT-Level II in PT,MT,RT & UT.
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Thu, Aug 23, 2018 at 11:53 AM Neem Lal <nee...@gmail.com> wrote:
Dear All,

We are doing fillet welding of 10 mm leg length, so throat should be around 7 mm.
But due to concave weld profile we are getting 4 mm  to 6 mm throat.

What are the possible remedies to rectify this.


Regards

Neem Lal
Welding Engineer
HMM INFRA LTD.
AMBALA (HR) 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...