Saturday, August 4, 2018

Re: [MW:28162] RE: 28154] PWHT required for HF service

Since the thk is more than 38 mm, PWHT is required irrespective of service as per Div.1.

Regards,
Ajay Pathak

On Sat, Aug 4, 2018 at 12:55 AM, PGoswami <pgoswami@quickclic.net> wrote:

If you're following API RP-751, then yes. Look at clause 3.3 of this RP, for guidance on PWHT for HF service. What's the precise service , HF Alkylation?? Ask your client to clarify.

 

Appreciate your response.

 

Thanks.

 

P.Goswami.P.Eng, IWE.

Welding & Metallurgical Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@quickclic.net,pradip.goswami@gmail.com

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Hrushikesh Sangamnerkar
Sent: August 1, 2018 1:48 AM
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:28154] PWHT required for HF service

 

Dear expert,

 

Query:

 

Service: HF

MoC: SA 516 Gr 70

P No. - 1

Thickness - 40mm

 

Is PWHT specifically required for HF service?

 

Client has not mentioned anything about Lethal or Sour service.

 

Pl suggest.

 

Regards,

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...