Dear Sir,
The answer is quite simple, DIN 18800-1 is already in 2010 replaced by EN 1993 part 1 so EN 1993 should be followed. EN 1993 part 1 is regarding engineering / design of structures. The Engineer responsible for the design need to calculate the structure and also throat thicknesses according to EN 1993 part 1 and should mention the required information on the drawing for production.
Met vriendelijke groeten / Best Regards,
Herman Pieper
QA-QC Inspector / CSWIP + IWI-C Welding Inspector / IWT / Materials Expert
Job van der Havestraat 6
8384 DB, Wilhelminaoord
Cell: +31 6 51691215
Van: 'Bijay' via Materials & Welding <materials-welding@googlegroups.com>
Verzonden: zaterdag 25 augustus 2018 11:11
Aan: Materials & Welding <materials-welding@googlegroups.com>
Onderwerp: [MW:28219] Throat Thickness in welding between DIN-18800 part 1 & EN1993 part 1
Dear Experts
In one of my project I have facing problems in throat thickness of welding.
Our governing code for welding is DIN - 18800 part 1, but as per clients instruction we have to follow the EN 1993 part 1 for throat thickness.
I can't find anything regarding throat thickness. Please guide what to do ?
Thank you in advance.
With Regards
Bijay Kumar Choudhury
Mob +91 8980630973
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Comments