Dear Experts,
-- We have repair in Golden joint and it is successfully done. But now client is asking for penalty for this joint as it was a 5% RT line.
But as per my understanding as it is a Golden Joint ( a 100% RT joint), so no need of repair penalty. But I am not getting any code reference to it. Please help me to find any reference.
Thanks and Regards,
Bishwambhar Kumar
Ph:- +974-55311582