Saturday, August 4, 2018

[MW:28161] RE: 28154] PWHT required for HF service

If you're following API RP-751, then yes. Look at clause 3.3 of this RP, for guidance on PWHT for HF service. What's the precise service , HF Alkylation?? Ask your client to clarify.

 

Appreciate your response.

 

Thanks.

 

P.Goswami.P.Eng, IWE.

Welding & Metallurgical Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@quickclic.net,pradip.goswami@gmail.com

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Hrushikesh Sangamnerkar
Sent: August 1, 2018 1:48 AM
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:28154] PWHT required for HF service

 

Dear expert,

 

Query:

 

Service: HF

MoC: SA 516 Gr 70

P No. - 1

Thickness - 40mm

 

Is PWHT specifically required for HF service?

 

Client has not mentioned anything about Lethal or Sour service.

 

Pl suggest.

 

Regards,

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...