Sunday, April 22, 2018

Re: [MW:27736] minimum distance limitation between two weld joints

I think that the minimum distance is to weld 3 times of thermal effective zone of first weld
  

2018-04-17 12:36 GMT+02:00 Kannayeram Gnanapandithan <kgpandithan@gmail.com>:
Ref BS EN 12952-5

On Tue 17 Apr, 2018 3:15 pm Veereswara Rao, <yeluguriveereswararao@gmail.com> wrote:
Hi Mr. Srirammadhan,
May I know the reference for the 1.5 times the outer dia as the minimum distance.

Regards,
Veereswara Rao Yeluguri.

On Tuesday, 6 March 2012 22:28:36 UTC+8, madhan wrote:
Hi 

the minimum spacing between two welds shall be 1.5 times the pipe OD or 5 times the pipe wall thickness whichever is greater.

regards,
madhan

On Tue, Mar 6, 2012 at 5:30 PM, murat aksoy <maks...@gmail.com> wrote:
Hello my friends,

I have a problem.

Is there minimum distance limitation between two weld joints as per ASME B31.3. or EN

thanks

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks & Regards
Srirammadhan
Piping/painting inspector
Great drill Chaaya
Great Ship
Hamriyah Free zone, UAE
+971-509846269

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...