Re: [MW:27728] Distance between two L-Seam

ASME Sect VIII Div 1 2017 Ed.: UW-9(d)

On Wed, Jun 13, 2012 at 9:24 PM, Gurunath.Hanamar <guru.h10@gmail.com> wrote:

Dear all,
I know that 100mm is permissble distance between two consecutive longitudinal seams but, can any one confirm minimum distance between two longitudinal seams should be mantained. Kindly mention ASME clause.

Thanks &Regards
Gurunath Hanamar

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...