[MW:27623] Reg. PQR

Dear Expert ,

As per ASME Sec. IX QW 203 - states that a qualification in any position qualifies the procedures for all position .

Now Can u all clarify one thing  , I  I have WPS in SMAW process and I am qualifying the PQR in 3G position , then according to above Clause it will be
qualified for position .

Whether its also applicable for 1G position also .

Pls. clarify briefly.


Thankyou 

S.Kharwar 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...