Tuesday, April 4, 2017

Re: [MW:26360] Galvanizing on flange face

Dear Mr Prasad rode,

Actually we have some spools that to be galvanized, galvanizing unit have done full spool galvanized with flange, my query is that whether flange face to protected or to be galvanized, please give  reference.

On Mon, Apr 3, 2017 at 5:45 PM, Prasad Rode <purode333@gmail.com> wrote:
Dear sir,

Why do you want to ganvanised the flanges?.

It is better to blast and paint it by protecting the serrations surface by brown tape/ mastic tape application.

Regards
Prasad

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/26ef2fcd-4bfd-4823-a8c5-0a1b106f90a1%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFycdMzqkxuimVaDJbxWM0gBULTLmL9rR9-rL1jyfkqHQAryKg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...