Saturday, April 1, 2017

Re: [MW:26331] RE: 26313] Hydro Test

Thanks for your valuable suggestion. 
 
Thanks & Regards, K.GANESAN Quality Control ISGEC / ISGEC John Thompson, A-4 Sector-24 Noida-201301 (UP) Tel. +91-120-2411175 Direct Tel. +91-120-2411175 Mobile : +91-9952166894


On Friday, 31 March 2017 10:27 PM, PGoswami <pgoswami@quickclic.net> wrote:


 
Pneumatic test is  not advisable for safety and integrity of piping components. Hence Hydro test is the default choice.
 
Hope it clarifies your doubt.
 
Thanks.
 
 
P.Goswami.P.Eng, IWE.
Welding & Metallurgical  Engineering Specialist
Email:pgoswami@quickclic.net,pradip.goswami@gmail.com
 
 
 
From: Ganesan [mailto:ganesandme03@yahoo.co.in]
Sent: March 30, 2017 7:25 AM
To: materials-welding@googlegroups.com; PGoswami <pgoswami@quickclic.net>; materials-welding@googlegroups.com
Subject: Re: [MW:26315] RE: 26313] Hydro Test
 
Noted for your valuable point. But the contractor is asking to show the code requirements. 
 
B31.1 has followed for design and fabrication of the Piping. 
 
 
On Thu, 30 Mar 2017 at 12:21 p.m., PGoswami
<pgoswami@quickclic.net> wrote:
What's the design and fabrication code for Piping??
 
Usually pressure piping  have to be hydro tested (by default) as like pressure vessel. No exceptions to rules?
 
A citation from the appropriate code or mentioning the appropriate code would be appreciated.
 
Thanks.
 
P.Goswami.P.Eng, IWE.
Welding&Metallurgical Specialist
Email:pgoswami@quickclic.net,pradip.goswami@gmail.com
 
From: 'Ganesan' via Materials & Welding [mailto:materials-welding@googlegroups.com]
Sent: March 29, 2017 6:13 AM
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:26313] Hydro Test
 
Dear Experts,
 
Could you please share the standard requirements for piping hydro test, because our chines contractor has not ready to conduct hydro test for the same piping. they said as per chines standard no need hydro test.
 
  
 
Thanks & Regards, K.GANESAN Quality Control ISGEC / ISGEC John Thompson, A-4 Sector-24 Noida-201301 (UP) Tel. +91-120-2411175 Direct Tel. +91-120-2411175 Mobile : +91-9952166894
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1216733524.5643000.1490782373350%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.
 

Image removed by sender. AVG logo
This email has been checked for viruses by AVG antivirus software.
www.avg.com


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAYAAAAAAAAAB/s9XS594ZCoMHlmX4xaZ3CgAAAEAAAADNg4iY9mnhIoxuiarCDI9UBAAAAAA%3D%3D%40quickclic.net.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAYAAAAAAAAAB/s9XS594ZCoMHlmX4xaZ3CgAAAEAAAABdWod%2B5UnRNoHYymn%2BJc9UBAAAAAA%3D%3D%40quickclic.net.
For more options, visit https://groups.google.com/d/optout.


No comments:

[MW:35725] Dismillar material Welding

Dear experts,  In my Hydro Electric Project  materials using A517Gr.F and A537CL-II.  For A517Gr.F using E 11018M and A537CL-II using E 9018...