Skip to main content

RE: [MW:26330] RE: 26313] Hydro Test

Pressure test is a mandatory requirement of  pressure piping designed and fabricated according to B-31.1 code. Clause 137 & various other clauses  of this code explicitly specifies the requirements. The medium could be Hydro or Pneumatic.

 

Pneumatic test is  not advisable for safety and integrity of piping components. Hence Hydro test is the default choice.

 

Hope it clarifies your doubt.

 

Thanks.

 

 

P.Goswami.P.Eng, IWE.

Welding & Metallurgical  Engineering Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@quickclic.net,pradip.goswami@gmail.com

 

 

 

From: Ganesan [mailto:ganesandme03@yahoo.co.in]
Sent: March 30, 2017 7:25 AM
To: materials-welding@googlegroups.com; PGoswami <pgoswami@quickclic.net>; materials-welding@googlegroups.com
Subject: Re: [MW:26315] RE: 26313] Hydro Test

 

Noted for your valuable point. But the contractor is asking to show the code requirements. 

 

B31.1 has followed for design and fabrication of the Piping. 

 

 

On Thu, 30 Mar 2017 at 12:21 p.m., PGoswami

<pgoswami@quickclic.net> wrote:

What's the design and fabrication code for Piping??

 

Usually pressure piping  have to be hydro tested (by default) as like pressure vessel. No exceptions to rules?

 

A citation from the appropriate code or mentioning the appropriate code would be appreciated.

 

Thanks.

 

P.Goswami.P.Eng, IWE.

Welding&Metallurgical Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@quickclic.net,pradip.goswami@gmail.com

 

From: 'Ganesan' via Materials & Welding [mailto:materials-welding@googlegroups.com]
Sent: March 29, 2017 6:13 AM
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:26313] Hydro Test

 

Dear Experts,

 

Could you please share the standard requirements for piping hydro test, because our chines contractor has not ready to conduct hydro test for the same piping. they said as per chines standard no need hydro test.

 

  

 

Thanks & Regards, K.GANESAN Quality Control ISGEC / ISGEC John Thompson, A-4 Sector-24 Noida-201301 (UP) Tel. +91-120-2411175 Direct Tel. +91-120-2411175 Mobile : +91-9952166894

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1216733524.5643000.1490782373350%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

 


This email has been checked for viruses by AVG antivirus software.
www.avg.com



--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAYAAAAAAAAAB/s9XS594ZCoMHlmX4xaZ3CgAAAEAAAADNg4iY9mnhIoxuiarCDI9UBAAAAAA%3D%3D%40quickclic.net.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...