Re: [MW:26199] ASME AND AWS D 1.1 clarification for wps qualificatioon

Dear Mr.Saravanan,

The choice of the code cannot be decided in this way.
This depend on your specification and the design code. This can be easily decided by a designer and should have a written documentation between the client, the Designer and the Contractor.

Regards,

Hareesh K V
8547859202

Dear Experts.

                      could we follow ASME section 9 or AWS D1.1  for the structural steel welding qualification? please explain.

--
K. SARAVANAN. BE, ME (WELDING TECHNOLOGY)
     WELDING ENGINEER,
     BLACKCAT ENGINEERING  WLL,
     DOHA ,QATAR.
     MOBILE: +974-77466433. INDIA- +91 8939999299.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALhxBzivrAMx4zTYJEtOb-jm6vEAxsVTm%3D%3DNrUNo6Z6s4Kme3Q%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM3LgAVCn0wPqfOqz3_f_%2BkhhPkgJ2vdjH9aywmEdi1ebRwyGw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...