CS is common which has got Low Carbon steel, Mild carbon steel, Medium carbon steel and high carbon steel.
It is based on %C
Low CS-----0.15max
MS---------- >0.15 to 0.35
Medium------>0.35 to 0.60
High ----------->0.60 to 1.00
THANKS & BEST REGARDS,
KG.PANDITHAN, IWE, AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349
On Tue, Mar 7, 2017 at 8:44 PM, Prasad Rode <purode333@gmail.com> wrote:
Dear sir,
This query with reference to trailing mail, which is for discussion mainly and also for knowledge sharing.
We all, always talking about M.S. plate and C.S. plate, like that what exactly it is?
Request all experts to give response to it.
Regards
Prasad Rode
--
http://www.linkedin.com/groups/MaterialsWelding- 122787?home=&gid=122787&trk= anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com .
To post to this group, send email to materials-welding@googlegroups.com .
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ .389580f1-f539-469d-8ee6- 6adebb3c5604%40googlegroups. com
For more options, visit https://groups.google.com/d/optout .
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eN-ZOumMKZ08x6-9EJCZgwyTzD1o4CMRPsraUqhqf38zg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
No comments:
Post a Comment