Tuesday, January 31, 2017

[MW:26009] Impact testing requirements for ASME B 31.3


Dear Experts,


Please clarify my below queries regarding the impact test requirements for Piping.


1) 3 inch SA105N WNRF  impact tested at zero degrees( at mill) Celsius but MDMDT is 18o Celsius can we use this flange with respect to ASME B 31.3( if yes please detail the reference standard and up to what temperature we can use this flange)


2) SA 234 GR WPB (90 degree elbow) MDMT is -450 Celsius but impact tested at Mill is -290 Celsius, can we use this flange with respect to ASME B 31.3.



Thanks and Best Regards?

D. Santosh
Tel: +971502016960
United Arab Emirates




No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...