Hi ,
Your query is not specific, What’s the base metal (substrate) and the hard facing alloy being considered for deposition? Could you be more specific?
Thanks.
Pradip Goswami, P.Eng,IWE
Welding & Metallurgical Engineering Specialist.
Ontario,Canada.
ca.linkedin.com/pub/pradip-goswami/5/985/299
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of AW
Sent: Monday, January 30, 2017 3:21 AM
To: Materials & Welding
Subject: [MW:26000] SAW hardfacing flux
I am struggling with hardness in my SAW hardfacing flux at present i use 68/8 HCFCR and still cant go beyond 52 HRC
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0f198d60-f2f1-4b2a-aa0b-f798239ca51c%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
No comments:
Post a Comment